Basic: Polyurethane Poglimer
Cutting mechanism: polymerization from moisture in the air
The formation of a surface film*: about 4 minutes
Curing speed*: about 60 minutes
Square area: from 1 m2
Flower thickness **: 50 mm
** The structure of the layer: finely/medium -porous
Distance from the nozzle of the applicator to the surface: 20 - 45 cm
Sound absorption coefficient: 55 dB
Breathability ***: & lt; 0.0045 kg/(m2 *hour)
Vapor perlife coefficient: 0.05 mg/(m*h*PA)
Water absorption coefficient1 % of the volume
Heater density: 19 - 25 kg/m3*
Surface temperature: from +5 to + 30 ° C
Using temperature: from +5 to + 30 ° C
Ballon temperature: from +18 to + 25 ° C
Thermal conductivity: 0.025 W/(m*K)
Possible expansion when heating: 20%
Thermal resistance: from - 80 to +115 ° C